PEMANFAATAN LIMBAH INDUSTRI BATU APUNG UNTUK PEMBUATAN BATU HIAS BANGUNAN

https://doi.org/10.22146/ajse.v1i1.2348

Arifin Hargianto(1*), Iman Satyarno(2), Mudjijana -(3)

(1) SMK N 2 Kuripan, Lombok Barat, Nusa Tenggara Barat
(2) Jurusan Teknik Sipil dan Lingkungan, Fakultas Teknik, Universitas Gadjah Mada
(3) Jurusan Teknik Mesin dan Industri, Fakultas Teknik, Universitas Gadjah Mada
(*) Corresponding Author

Abstract


Mining and processing activities have caused pumice deposits of waste. Waste from industrial processing of pumice is used as an innovation to increase the value of the waste and then profits will be obtained. One of the examples is making them as decorative stones.

Raw materials used in this study are industrial waste pumice from Lombok, with the size less than 2 cm. The machine used as a fine aggregate pumice waste destruction is a crusher. Variations of the composition of the mixed mortar are made from white cement, powdered pumice waste as fine aggregate, and water. Variation is the comparison between the composition of the mixture of white portland cement (pc) and fine aggregate from pumice waste (Ag.h) with comparisons 1Pc: 2Ag.h, 1Pc: 4Ag.h, 1Pc: 6Ag.h, 1Pc: 8Ag.h and 1Pc: 10Ag.h. Tests are conducted to determine the characteristics of fine aggregate made from pumice waste, while the mortar test includes compressive strength, flexural strength, specific gravity and water absorption.

The results show that the fine aggregate made from pumice industrial waste materials has the following characteristics : modulus of fine grains is 2.61, specific gravity is 1.67, absorption of water is 23.08%, mud content is 26.10%, and weight lose unit is 0.537 gr/cm3. On the mortar test, mixed variations affect the compressive strength, flexural strength, specific gravity and water absorption. The test results find that the variation of a mixture of 1 pc: 2 Ag.h has characteristics of natural stone that is the closest to the gravity of 262 gr/cm and with 3,11 813 MPa in compressive strength, 0344 MPa in flexural strength, and 19.93% in water absorption value. Variation of a mixture of 1 pc: 2 Ag.h has also been tested in the manufacture of decorative stones and the results can have the similar look with the natural stone.

Keywords


Decorative Stones; Pumice Waste; Mortar

Full Text:

PDF


References

Mulyono, T., 2005, Teknologi Beton, Penerbit Andi, Yogyakarta.

Satyarno, I., 2004, Penggunaan Semen Putih Untuk Beton Styrofoam Ringan, Program S1 Ekstensi Jurusan Teknik Sipil Fakultas Teknik, UGM, Yogyakarta.

Solehuddin, 2011, Kreasi Unik Batu Alam, Griya Kreasi, Jakarta.

Tjokrodimuljo, K., 2010, Teknologi Beton, Biro Penerbit KMFTS FT UGM, Yogyakarta.



DOI: https://doi.org/10.22146/ajse.v1i1.2348

Article Metrics

Abstract views : 1113 | views : 4183

Refbacks

  • There are currently no refbacks.


Copyright (c)




ASEAN Journal of Systems Engineering (AJSE) 
P-ISSN: 2338-2309 || E-ISSN: 2338-2295
Master in Systems Engineering
Faculty of Engineering
Universitas Gadjah Mada
Jl. Teknika Utara No.3, Barek, Yogyakarta, Indonesia 55281 
Website: https://journal.ugm.ac.id/ajse
Email: jurnalajse@gmail.com | ajse@ugm.ac.id